Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 3700 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 25.5 GPa

@Temperature 23.9 °C
3700 ksi

@Temperature 75.0 °F
0° Direction, Dry; Oven Cure 250°F, 90 min; ASTM D3039
Park Electrochemical Nelcote® E-763 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-763 is a modified epoxy system with a nominal 250°F cure temperature. E-763 provides a transparent resin surface on the finished part which gives finished part surfaces a cosmetic attra..
Tensile Modulus 25.5 GPa

@Temperature 23.9 °C
3700 ksi

@Temperature 75.0 °F
0° Direction, Dry; ASTM D638 Type 1
Park Electrochemical Nelcote® V-303 Polyimide Prepreg, 7781 E-Glass Reinforced
Nelcote® V-303 is non-MDA condensation polyimide prepreg with a service temperature of 600°F.Key Features and Benefits:600°F maximum service temperatureGood electrical properties for RF applicati..
Tensile Modulus 25.5 GPa

@Temperature 23.9 °C
3700 ksi

@Temperature 75.0 °F
0° Direction, Dry; ASTM D638
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 581 Quartz Reinforced
Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low ..
Tensile Modulus 25.5 GPa
3700 ksi
ASTM D638
Sumitomo Bakelite Sumikon® PM-9610 Glass-Filled Phenolic, Compression Grade
Sumikon PM-9610 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and higher dimens..
Tensile Modulus 25.5 GPa
3700 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® GVX-65 H black 9915 PA*-GF65
Product description: Grivory GVX-65H black 9915 is a 65% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolya..
Tensile Modulus 25.5 GPa
3700 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® GVX-65 H nat PA*-GF65
Product description: Grivory GVX-65H natural is a 65% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyami..
Tensile Modulus 25.5 GPa
3700 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® HT1V-65H black 9205 PA6T/6I-GF65
Product description: Grivory HT1V-65H black 9205 is a 65% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I..
Tensile Modulus 25.5 GPa
3700 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® HT1V-65H black 9205 PA6T/6I-GF65
Product description: Grivory HT1V-65H black 9205 is a 65% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I..
Copyright © lookpolymers.com All Rights Reserved