Polymer Property : Tensile Modulus = 376.8 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.598 GPa
376.8 ksi
ASTM D638
SABIC PS 126 General Purpose Polystyrene for Injection Molding
Product Description: General purpose Polystyrene PS 125 is manufactured by continuous mass polymerization of styrene monomer. It is a crystal-like, hard and brittle polymer with medium flow and hi..