Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.62 GPa | 380 ksi | ASTM D638 |
Polymer Resources ABS-GP1 General Purpose ABS General Purpose Acrylonitrile Butadiene StyreneFeatures: • Medium Impact ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | ASTM D638 |
Polymer Resources ABS-GP1-[color]-EP General Purpose ABS, Electroplating Grade General Purpose Acrylonitrile Butadiene Styrene, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Dry Blend E7001 Polyvinyl Chloride, Rigid (PVC, Rigid) 60 degree gloss comparisons: Geon E7001 is 27-29; Geon E7456 is 40-49; Geon E7130 is 38-43; Geon E7370 is 26-31Information provided by PolyOne |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | ASTM-D638 |
Ineos ABS Lustran® ABS 349 Lustran® ABS 349 is a high-gloss, medium-impact injection molding resin that has been specially formulated for excellent surface lubricity using internal additives. |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | ASTM-D638 |
Ineos ABS Lustran® Guardian™ 620 ABS, Extrusion Grade Lustran® Guardian™ ABS 620 is a high modulus, HFC 134a and HCFC 22 resistant extrusion grade resin designed for refrigerator door and food liners. Lustran® ABS 620 offers good melt streng.. |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DD0009P PC (Asia Pacific) LNP STAT-KON* DD0009P is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DX05305C PC (Asia Pacific) LNP* Stat-kon* DX05305C is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Clean Compounding System. |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp MH0500A PP (Asia Pacific) LNP THERMOCOMP* MH0500A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL N850 PPE+PS ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications. |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL N850 PPE+PS (Asia Pacific) ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications. |
|||
Tensile Modulus | 2.62 GPa @Thickness 3.20 mm |
380 ksi @Thickness 0.126 in |
Injection Molded; ASTM D638 |
Styron EMERGEâ„¢ 7700 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) Overview: EMERGEâ„¢ PC/ABS 7700 Advanced Resin is an ignition-resistant PC/ABS blend that contains no chlorine for bromine additives. It has superior processability for injection molding applicat.. |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | ASTM D638 |
Westlake Plastics Pomalux® Acetal Copolymer, Compression Molded Compression molded Pomalux is a high performance acetal copolymer with excellent mechanical, electrical, and wear properties. Pomalux has excellent dimensional stability even with complex geometrie.. |
|||
Tensile Modulus | 2.62 - 2.74 GPa | 380 - 397 ksi | ASTM D638M |
DSM Somos® ProtoGen™ O-XT 18120 Epoxy Resin for Stereolithography, UV Postcure at HOC -2 DescriptionDSM Somos® ProtoGen O-XT 18120 is a liquid photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demonstrate diffe.. |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | ASTM D-638 |
Axiall 7140 Rigid PVC, Extrusion & Molding Georgia Gulf 7140 is a special purpose rigid PVC compound designed for applications requiring the following properties: WeatherabilityGlossImpact Strength & ToughnessFlame RetardantChemical Resista.. |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | ASTM D-638 |
Axiall CL-7053 Rigid PVC, Molding Georgia Gulf CL-7053 is a clear, high flow vinyl compound designed for a variety of end-use molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | ASTM D-638 |
Axiall SP-7107 Rigid PVC, Molding Georgia Gulf SP-7107 is a general purpose, electrical grade rigid vinyl injection molding compound characterized by excellent flow, heat stability, color hold and surface appearance. This makes it .. |
|||
Tensile Modulus | 2.62 GPa @Temperature 120 °C |
380 ksi @Temperature 248 °F |
ISO Data |
BASF Ultramid® 8267G HS BK-106 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-106 is a heat stabilized, weather resistant, 40% mineral and glass fiber reinforced PA6 injection molding compound with improved UV resistance and sink mark resistance. The com.. |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | ASTM D-638 |
Axiall 8247 Clear 34 Rigid PVC, Extrusion, Clear 34 Georgia Gulf 8247 Clear 34 is a rigid PVC pellet compound suited for applications where transparency is important. It is widely used for clear profiles such as furniture trim, shower door and prote.. |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | ASTM D638 |
Asahi Kasei Thermylene® F6-10FG-0100 10% Glass Fiber Reinforced, Chemically Coupled Information provided by Asahi Thermofil |
|||
Tensile Modulus | 2.62 GPa | 380 ksi | ASTM D-638 |
Axiall 3240 Rigid PVC, Extrusion Georgia Gulf 3240 is a special purpose rigid powder blend PVC compound designed for applications requiring the following properties: WeatherabilityGlossImpact Strength & ToughnessFlame RetardantChe.. |