Polymer Property : Tensile Modulus = 391 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.70 GPa
391 ksi
ISO 527
FKuR Kunststoff Biograde® C 6509 CL Biodegradable Plastic Compound
BIOGRADE® are easy to process blends based on cellulose. BIOGRADE® is composed mainly of natural resources. Based on cellulose, a product of the paper industry BIOGRADE® has been especial..