Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 26.96 GPa | 3910 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON RE0069S PA 66 LNP* STAT-KON* RE0069S is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Heat Stabilized. |