Mechanical Properties Metric English Comments
Tensile Modulus 4.28 GPa
621 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DFL32 PC
LNP LUBRICOMP* DFL32 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 15% PTFE. Added features of this material include: Internally Lubricated.
Tensile Modulus 4.28 GPa
621 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DFL32XXC PC
LNP LUBRICOMP* DFL32XXC is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated.
Tensile Modulus 4.28 GPa
621 ksi
ISO 527
Polyram RamOfin PPH501G4 Polypropylene, 20% Glass Fiber, Flame Retardant
Glass fiber 20% reinforced, halogen free, flame retardant polypropylene for injection molding applications.Information provided by Polyram.