Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.71 GPa | 683 ksi | ISO 527 |
Ineos ABS Lustran® SAN DN59 SAN, Soft-Flow Grade Lustran® SAN DN59 resin is a soft-flow grade of transparent SAN (styrene acrylonitrile) thermoplastic. It has been designed for use in compounding and thin-wall injection molded applications. Lus.. |