Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.00 - 4.80 GPa @Thickness 4.00 mm, Temperature 23.0 °C |
580 - 696 ksi @Thickness 0.157 in, Temperature 73.4 °F |
depending on color; ISO 527-2/1 |
PolyOne Bergamid™ A70 GK30 H Polyamide 66 (Nylon 66) Information provided by PolyOne |