Polymer Property : Tensile Modulus = 4.88 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 4.88 GPa
708 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP 9X02841 PBT+PC
LNP* Thermocmop* 9X02841 is a PBT/Polycarbonate blend containing proprietary fillers.
Tensile Modulus 4.88 GPa

@Temperature 70.0 °C
708 ksi

@Temperature 158 °F
DAM; Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66  (Unverified Data**)
40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P..