Tensile Modulus 400 GPa
58000 ksi
Young's; DINV ENV 843-2 / ASTM-F417
CeramTec 433 Alumina, 99.9%
433 (99.9%) is an alumina that exhibits high hardness. Its fine, equiaxial microstructure provides excellent sliding and abrasive wear resistance. This material is ideal for corrosive conditions. A ..