Mechanical Properties Metric English Comments
Tensile Modulus 2.41 - 2.76 GPa
350 - 400 ksi
Master Bond EP42HT-2Med Epoxy Meets USP Class VI Requirements
Description: Master Bond Polymer System EP42HT-2Med is a room temperature curable two component epoxy, adhesive, sealant, coating and casting material featuring high temperature resistance along wit..
Tensile Modulus 2.41 - 2.76 GPa

@Temperature 23.9 °C
350 - 400 ksi

@Temperature 75.0 °F
Master Bond EP21LSCL-1 Two Component, Room Temperature Curing Epoxy Resin
Product Description: Master Bond Polymer System EP21LSCL-1 is a two component, low viscosity epoxy resin system featuring optical clarity as well as non-yellowing properties. This system can be used..
Tensile Modulus 2.41 - 2.76 GPa
350 - 400 ksi
Master Bond EP30M4 Chemically Resistant Two Component Epoxy System
Master Bond Polymer System EP30M4 is a two component epoxy system for high performance bonding, sealing and encapsulation. This system features a forgiving 100 to 60 mix ratio by weight. EP30M4 resi..
Tensile Modulus 2.41 - 2.76 GPa
350 - 400 ksi
Master Bond EP42HT-2 Epoxy Adhesive Resists Sterilization
Description: Master Bond Polymer System EP42HT-2 is a room temperature curable, two component epoxy adhesive, sealant, coating and casting material featuring high temperature resistance along with o..