Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 276 GPa | 40000 ksi | Typical fiber property; Chord 6000-1000 |
Hexcel® HexTow™ IM7 (5000) Carbon Fiber HexTow™ IM7 (HS-CP-5000) carbon fiber is a continuous, high performance, intermediate modulus, PAN based fiber available in 6,000 (6K) and 12,000 (12K) filament count tows. The fiber has been surfa.. |
|||
Tensile Modulus | 276 GPa | 40000 ksi | Young's; DINV ENV 843-2 / ASTM-F417 |
CeramTec 614/698 Alumina, 96% 614/698 (96%) is a high-strength alumina with good mechanical properties, as well as good wear and chemical resistance. It also features excellent electrical properties. 614 is white; 698 is pink. |