Mechanical Properties Metric English Comments
Tensile Modulus 2.896 GPa
420.0 ksi
ASTM D638
Resirene Resirene® HH-104 General Purpose Polystyrene
Features:Medium FlowHigh HeatHigh Molecular WeightExternal LubricationFDA Rating: 21 CFR 177.1640Mold ReleaseApplications:InjectionPen BarrelsCassettesInformation provided by US distributor Calsak C..
Tensile Modulus 2.896 GPa
420.0 ksi
XY; ASTM D638
ALM PA 601-CF Filled Nylon 12 Prototyping Polymer
Carbon fiber filled nylon 12 easy to process, strong light weight filled material.Low density, good dimensional stability while maintaining excellent mechanical properties.Fibers have been optimized..
Tensile Modulus 2.896 GPa
420.0 ksi
ASTM D638
Resirene Resirene® HF-666 General Purpose Polystyrene
Features:High FlowEasy ProcessingHigh ProductivityFDA Rating: 21 CFR 177.1640External Lubrication AvailableApplications:Medium Wall ApplicationsInjectionToysCassette CasesInformation provided by US ..