Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.98 GPa | 432 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp KI001A Acetal LNP* Lubricomp Fulton 441D is an Acetal based compound with Silicone.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.98 GPa | 432 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DX04490 PC LNP* STAT-KON* DX04490 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
Tensile Modulus | 2.98 GPa | 432 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP MF002S PP LNP* Thermocomp* MF002S is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 2.98 GPa | 432 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DX04490 PC (Asia Pacific) LNP* Stat-kon* DX04490 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |