Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.007 GPa | 436.1 ksi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers NPP25-0120B GF15 Glass Filled Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Modulus | 3.007 GPa @Temperature 60.0 °C |
436.1 ksi @Temperature 140 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G15L NC010 Nylon 6
(Unverified Data**) 15% Glass Reinforced Polyamide 6Zytel 73G15L NC010 is a 15% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |