Mechanical Properties Metric English Comments
Tensile Modulus 30.1 GPa
4370 ksi
longitudinal; ISO 527-4/5
Bond Laminates TEPEX® dynalite 102-RGUD600(x)/47% Roving Glass – PA 6 Consolidated Composite Laminate
Within the TEPEX® composite laminate, Polyamide 6 is a resin known for its toughness, stiffness, abrasion resistance, heat and chemical resistances. Roving E-Glass fibers have an excellent impact ..