Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.15 GPa | 457 ksi | ISO 527-1/-2 |
Quadrant EPP Nylatron® NSM PA 6 + internal lubricant, cast (ISO Data) Nylatron NSM is a proprietary cast nylon 6 formulation containing solid lubricant additives which grant this materials self-lubricity, excellent frictional behaviour, superior wear resistance and ou.. |
|||
Tensile Modulus | 3.15 GPa | 457 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® DMX9254 PC Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl.. |
|||
Tensile Modulus | 3.15 GPa | 457 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® DMX9254 PC (Asia Pacific) Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl.. |
|||
Tensile Modulus | 3.15 GPa | 457 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® DMX9254 PC (Europe-Africa-Middle East) Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl.. |
|||
Tensile Modulus | 3.15 GPa | 457 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Tensile Modulus | 3.15 GPa | 457 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Asia Pacific) LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Tensile Modulus | 3.15 GPa | 457 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Europe-Africa-Middle East) LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Tensile Modulus | 3.15 GPa | 457 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 LNP* FARADEX* PS003E is a compound based on Nylon 6 resin containing 15% Stainless Steel. Added features of this material include: EMI/RFI Shielding. |
|||
Tensile Modulus | 3.15 GPa | 457 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 (Asia Pacific) LNP* Faradex* PS003E is a compound based on Nylon 6 resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Tensile Modulus | 3.15 GPa | 457 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 (Europe-Africa-Middle East) LNP* Faradex* PS003E is a compound based on Nylon 6 resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Tensile Modulus | 3.15 GPa | 457 ksi | ISO 527 |
FKuR Kunststoff Biograde® C 6530 Biodegradable Plastic Compound BIOGRADE® are easy to process blends based on cellulose. BIOGRADE® is composed mainly of natural resources. Based on cellulose, a product of the paper industry BIOGRADE® has been especial.. |
|||
Tensile Modulus | 3.15 GPa | 457 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl TN240 PPE+PS PPE+PS blend. Unfilled. Transparent. Good flow. Scratch resistant. Injection molding. Suitable for housewares, personal care and small appliance applications.This data was supplied by SABIC-IP for t.. |
|||
Tensile Modulus | 3.15 GPa | 457 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl TN240 PPE+PS (Asia Pacific) PPE+PS. Transparent. High flow, scratch resistant. Injection molding. Housewares and small appliances applications.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 3.15 GPa | 457 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP IAL12 PA 6/12 (Asia Pacific) LNP* Lubricomp* IAL12 is a compound based on Nylon 6/12 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 3.15 GPa | 457 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® ENH3500 PBT (Asia Pacific) Unfilled PBT, Non-Brominated & Non-Chlorinated Flame Retardant |
|||
Tensile Modulus | 3.15 GPa | 457 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® ENH3500 PBT (Europe-Africa-Middle East) Unfilled PBT, Non-Brominated & Non-Chlorinated Flame Retardant |
|||
Tensile Modulus | 3.15 GPa | 457 ksi | ISO 527-1/-2 |
DSM Akulon® F136-DH Nylon 6 (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 3.15 GPa | 457 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 111DP NC010 Acetal (POM)
(Unverified Data**) Nucleated High Viscosity Acetal Homopolymer Delrin 111DP is a new high viscosity acetal homopolymer with enhanced crystallization and excellent creep and fatigue resistance. It has improved thermal .. |
|||
Tensile Modulus | 3.15 GPa | 457 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® II150E BK602 Acetal (POM) Nucleated High Viscosity Acetal Homopolymer Developed for ExtrusionInformation provided by DuPont Performance Polymers |
|||
Tensile Modulus | 3.15 GPa | 457 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Tensile Modulus | 3.15 GPa | 457 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 100 NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Tensile Modulus | 3.15 GPa | 457 ksi | 1 mm/min; ISO 527 |
Polimeri Europa Edistir N 2982 Polystyrene General purpose polystyrene with very high flow and high heat resistance. Special grade for direct gassing extrusion of heavy gage insulating boards (XPS) foamed by blowing agents alternative to CFC.. |