Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 32.75 GPa | 4750 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON OE006A PPS - Branched LNP STAT-KON* OE006A is a compound based on PPS - Branched resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |