Mechanical Properties Metric English Comments
Tensile Modulus 5.33 GPa
773 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® BFL2015 PC
Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only
Tensile Modulus 5.33 GPa
773 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® BFL2015 PC (Asia Pacific)
Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only
Tensile Modulus 5.33 GPa
773 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® BFL2015 PC (Europe-Africa-Middle East)
Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only
Tensile Modulus 5.33 GPa
773 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® BFL2015HF PC (Asia Pacific)
Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only. UL94 V0 1.5 mm for BLACK; V1 1.5 mm for OTHER Color.
Tensile Modulus 5.33 GPa
773 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DFL23 PC (Asia Pacific)
LNP* Lubricomp* DFL23 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Tensile Modulus 5.33 GPa
773 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DFL23 PC
LNP* Lubricomp* DFL23 is a compound based on Polycarbonate resin containing 15% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated.
Tensile Modulus 5.33 GPa
773 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1040 PP
SABIC® PPcompound 19T1040 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding application..