Tensile Modulus 5.63 GPa
817 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® ML7672 PC (Asia Pacific)
Non FR PC + GF, UV-Stabilizer, balanced flow & impact. Available in Opaque only.
Tensile Modulus 5.63 GPa
817 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP RFL32 PA 66
LNP* Lubricomp* RFL32 is a compound based on Nylon 66 containing 10% Glass Fiber, 15% PTFE. Added feature of this material includes: Wear Resistant.
Tensile Modulus 5.63 GPa
817 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP PH0240A PA 6
LNP* THERMOCOMP* PH0240A is a compound based on Nylon 6 resin. Added features of this grade include: High Impact, High Specific Gravity.