Polymer Property : Tensile Modulus = 5.81 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 5.81 GPa
843 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP MX06404 PP (Asia Pacific)
LNP* LUBRICOMP* MX06404 is a compound based on Polypropylene resin containing PTFE, Glass Fiber. Added features of this material include: Heat Stabilized.