Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.97 GPa | 866 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Faradex EX06464 PEI (Asia Pacific) LNP* Faradex* EX06464 is a compound based on Polyetherimide resin containing Stainless Steel. Added features of this material include: Electrically
Conductive, EMI/RFI Shielding.This data was suppli.. |
|||
Tensile Modulus | 5.97 GPa | 866 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RF002 PA 66 LNP THERMOCOMP* RF002 is a compound based on Nylon 66 resin containing 10% Glass Fiber. |