Polymer Property : Tensile Modulus = 505.7 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 3.487 GPa
505.7 ksi
Type 1B, 50mm/min; ISO 527-1/2:1993
Nylacast H.S. Blue Cast Nylon 6, Heat Stabilized
HS Blue is a heat Stabilised Cast Nylon 6. Its mechanical properties are maintained when operating at higher temperature and improves mechanical properties. This helps to reduce the stress distortio..