Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 35.25 GPa | 5113 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON RE0069S PA 66 (Asia Pacific) LNP* STAT-KON* RE0069S is a compound based on Nylon 66 resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Heat Stabil.. |