Mechanical Properties Metric English Comments
Tensile Modulus 3.64 GPa
528 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RL0019 PA 66
LNP LUBRICOMP* RL0019 is a compound based on Nylon 66 resin containing 5% PTFE. Added features of this material include: Flame Retardant, Wear Resistant.
Tensile Modulus 3.64 GPa
528 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP ZFL31XXC PPE+PS
LNP* LUBRICOMP* ZFL31XXC is a compound based on PPE+PS resin containing 5% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant
Tensile Modulus 3.64 GPa
528 ksi
1 mm/min
Arkema Group Rilsan® AUM 50 NOIR T6LD Nylon 12, 50% Glass Bead Filled (Dry)
Designation ISO 1874-PA12,MHLR,16-020,GB50Rigid grad with glass beads filler (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agents. Mold-release agent.Goo..