Tensile Modulus 3.684 GPa

@Temperature 60.0 °C
534.3 ksi

@Temperature 140 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK603 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
20% Glass Reinforced Polybutylene Terephthalate Crastin SK603 NC010 is a 20% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P..