Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 535 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 3.69 GPa
535 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON EX01696C PEI
LNP* STAT-KON* EX01696C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System.
Tensile Modulus 3.69 GPa
535 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON EX01696C PEI (Asia Pacific)
LNP* Stat-kon* EX01696C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System.
Copyright © lookpolymers.com All Rights Reserved