Polymer Property : Tensile Modulus = 55.1 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 55.1 GPa
7990 ksi
ASTM D638
Quantum Composites Lytex® 4149 55% Carbon Fiber Epoxy SMC
Lytex 4149 is a high-performance, 3K tow carbon fiber (PAN) reinforced epoxy sheet molding compound designed for military and aerospace structural applications requiring excellent mechanical propert..