Polymer Property : Tensile Modulus = 563 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 3.88 GPa
563 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP CZL36 PS
LNP LUBRICOMP* CZL36 is a compound based on Polystyrene resin containing 30% Milled Glass and 15% PTFE. Added features of this material include: Internally Lubricated.