Polymer Property : Tensile Modulus = 580.1 ksi
Polymer Property :
Tensile Modulus =
580.1 ksi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Modulus
4.000
GPa
580.1
ksi
ASTM D638
Aclo Accutech ABS ABS833G20L Glass Reinforced
Tensile Modulus
4.000
GPa
580.1
ksi
ASTM D638
Aclo Accutech Polypropylene Copolymer CP0436G40CL Glass Reinforced
Tensile Modulus
4.000
GPa
580.1
ksi
ASTM D638
Aclo Accutech Polypropylene Copolymer CP0437G40CL Glass Reinforced Coupled
Tensile Modulus
4.000
GPa
580.1
ksi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0339G30CL Glass Reinforced Coupled
Tensile Modulus
4.000
GPa
580.1
ksi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0339W40L1 Wollastonite Reinforced
Tensile Modulus
4.000
GPa
580.1
ksi
ASTM D638
Aclo Accutech ABS ABS831G20L Glass Reinforced
Tensile Modulus
4.000
GPa
580.1
ksi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0336G30CL Glass Reinforced Coupled
Tensile Modulus
4.000
GPa
580.1
ksi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0339M30CL Mica Reinforced Coupled
Tensile Modulus
4.000
GPa
580.1
ksi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0339M40CL Mica Reinforced Coupled