Mechanical Properties Metric English Comments
Tensile Modulus 6.23 GPa
904 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP WH0200B PBT
LNP* Thermocomp* WH0200B is a compound based on PBT resin containing proprietary fillers. Added features include: High Specific Gravity.
Tensile Modulus 6.23 GPa
904 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Verton RV004ESV_GY7E070 PA 66
Preliminary data for 20% long glass fiber filled, single pellet color gray, PA66This data was supplied by SABIC-IP for the Americas region.