Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.55 GPa | 950 ksi | |
Plastcom SLOVAMID 66 T 36 TS PA66, 36% mineral filling FeaturesPA 66 with the content of 36 % chemically modified mineral filling. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat products, automobile wheel.. |
|||
Tensile Modulus | 6.55 GPa | 950 ksi | |
Zelfo Technology Zelfo® HZ Cellulose Fiber Material Zelfo® is a high performance bio-based material. Patented fibre technology developed by Zelfo Technology transforms 100% renewable or recycled cellulose fibres and water into self-binding Zelfo mat.. |
|||
Tensile Modulus | 6.55 GPa | 950 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AS-30GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 6.55 GPa | 950 ksi | ASTM D1708 |
Solvay Specialty Polymers Torlon® 4301 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4301 is a wear-resistant grade of polyamide-imide (PAI) resin. It has a good balance of mechanical properties and wear resistance. It offers high flexural and compressive strength with a low .. |
|||
Tensile Modulus | 6.55 GPa | 950 ksi | ASTM D638 |
Fiberfil® J-61/30/FR Polypropylene Copolymer, 30% Glass Reinforced, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 6.55 GPa | 950 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DX00714H PC LNP LUBRICOMP* DX00714H is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Wear Resistant, Healthcare. |
|||
Tensile Modulus | 6.55 GPa | 950 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DX00714H PC (Asia Pacific) LNP LUBRICOMP* DX00714H is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 6.55 GPa | 950 ksi | ASTM D638 |
Techmer ES Electrafil® M-2426 BK Polycarbonate |
|||
Tensile Modulus | 6.55 GPa | 950 ksi | ASTM D638 |
Solvay Specialty Polymers Torlon® 4301 Polyamide-imide (PAI) Torlon® 4301 is a wear-resistant grade of polyamide-imide (PAI) resin. It has a good balance of mechanical properties and wear resistance. It offers high flexural and compressive strength with a .. |
|||
Tensile Modulus | 6.55 GPa | 950 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP SF006 PA 12 LNP THERMOCOMP* SF006 is a compound based on Nylon 12 resin containing 30% Glass Fiber. |
|||
Tensile Modulus | 6.55 GPa | 950 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp SF006S PA 12 LNP* Thermocomp* SF006S is a compound based on Nylon 12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re.. |
|||
Tensile Modulus | 6.55 GPa | 950 ksi | ASTM D638 |
LNP Thermocomp® SF-1006 Polyamide 12, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |