Mechanical Properties Metric English Comments
Tensile Modulus 6.69 GPa

@Temperature 100 °C
970 ksi

@Temperature 212 °F
ISO 527-2
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi..
Tensile Modulus 6.69 GPa
970 ksi
Conditioned; ASTM D638
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. Th..
Tensile Modulus 6.69 GPa
970 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics SABIC STAMAX 30YM240 PP
SABIC® STAMAX 30YM240 is a 30% long glass fiber reinforced polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS is 16496906...
Tensile Modulus 6.69 GPa
970 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics SABIC STAMAX 30YM243 PP
SABIC® STAMAX 30YM243 is a 30% long glass fiber reinforced UV stabilized polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMD..
Tensile Modulus 6.69 GPa

@Temperature 100 °C
970 ksi

@Temperature 212 °F
2; ISO 527-2
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Dry)
Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s..
Tensile Modulus 6.69 GPa
970 ksi
ASTM D638
Asahi Kasei Thermylene® P6-43FG-0410 43% Glass Fiber Reinforced, Heat and UV Stabilized
Information provided by Asahi Thermofil
Copyright © lookpolymers.com All Rights Reserved