Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.93 GPa | 1010 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON MX01739C PP LNP* SAT-KON* MX01739C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System. |
|||
Tensile Modulus | 6.93 GPa | 1010 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP LF003 PEEK LNP* THERMOCOMP* LF003 is a compound based on Polyetheretherketone resin containing 15% Glass Fiber. |
|||
Tensile Modulus | 6.93 GPa | 1010 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP LF003 PEEK (Asia Pacific) LNP* Thermocomp* LF003 is a compound based on Polyetheretherketone resin containing Glass Fiber. |
|||
Tensile Modulus | 6.93 GPa | 1010 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp LF003E PEEK LNP* Thermocomp* LF003E is a compound based on Polyetheretherketone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 6.93 GPa | 1010 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp LF003E PEEK (Asia Pacific) LNP* Thermocomp* LF003E is a compound based on Polyetheretherketone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 6.93 GPa | 1010 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP VERTON MV006BS PP LNP* VERTON* MV006BS is a compound based on Polypropylene resin containing 30% Long Glass Fiber. Added features of this grade include: Heat Stabilized, Burst Pressure, Structural, Chemically Coupl.. |