Mechanical Properties Metric English Comments
Tensile Modulus 0.443 GPa

@Temperature 150 °C
64.3 ksi

@Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 73M30 NC010 Nylon 6  (Unverified Data**)
30% Mineral Reinforced Polyamide 6 Minlon 73M30 NC010 is a 30% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro..