Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.15 GPa | 1040 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp OF002A PPS LNP* Thermocomp* OF002A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 7.15 GPa | 1040 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp OF002A PPS (Asia Pacific) LNP* Thermocomp* OF002A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 7.15 GPa | 1040 ksi | ASTM D638 |
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness) AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |