Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.28 GPa | 1060 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36G PC LNP* Lubricomp* DFL36G is a compound based on Polycarbonate resin containing 30% Mixed Glass, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 7.28 GPa | 1060 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP JF004LZ PES LNP* Thermocomp* JF004LZ is a compound based on PES containing 20% Glass Fiber. Added features include: Extrusion Grade, Low Extractible. |
|||
Tensile Modulus | 7.28 GPa | 1060 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RB006 PA 66 LNP* THERMOCOMP* RB006 is a compound based on Nylon 66 resin containing 30% Glass Bead. |
|||
Tensile Modulus | 7.28 GPa | 1060 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36G PC (Asia Pacific) LNP* Lubricomp* DFL36G is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Milled Glass. Added features of this material include: Internally Lubricated. |