Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.57 GPa | 1100 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp PFL34 PA 6 LNP* Lubricomp* PFL34 is a compound based on Nylon 6 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Am.. |
|||
Tensile Modulus | 7.57 GPa | 1100 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp PFL34 PA 6 (Asia Pacific) LNP* Lubricomp* PFL34 is a compound based on Nylon 6 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the As.. |
|||
Tensile Modulus | 7.57 GPa | 1100 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DC10EPFR PC LNP* STAT-KON* Lexan_DC10EPFR is a compound based on Polycarbonate containing Carbon Fiber. Added features of this grade include: Exceptional Processing, Flame Retardant, Electrically Conductive. |