Polymer Property : Tensile Modulus = 703 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 4.85 GPa
703 ksi
Plastcom SLOVASTER® B1 GF 10 FRX 5 PBT reinforced with 10% glass fibre, with flame retardant
Features: PBT with the content of 10 % chemically bound glass fibre and with the halogen freeflame retardant. Anisotropy of shrinkage enables the injection moulding of round, cylindrical or other ho..
Tensile Modulus 4.85 GPa
703 ksi
Plastcom SLOVAMID 6 GF 15 HI PA6, 15% glass fibre, improved strength
FeaturesPA 6 for injection moulding, chemically strengthened with 15% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and..
Tensile Modulus 4.85 GPa
703 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RF002ES PA 66
LNP THERMOCOMP* RF002ES is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
Tensile Modulus 4.85 GPa
703 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP MF742XXH PP
LNP* THERMOCOMP* MF742XXH is a compound based on Polypropylene resin containing Glass Fiber and proprietary antimicrobial additives. This product is best suited for touch surfaces in healthcare app..