Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 71.0 GPa @Temperature 21.1 °C |
10300 ksi @Temperature 70.0 °F |
0° Direction, Dry; Autoclave Cured; ASTM D3039-95 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 34-700 12K 2x2 Twill Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Tensile Modulus | 71.0 GPa @Temperature 21.1 °C |
10300 ksi @Temperature 70.0 °F |
0° Direction, Dry; Vacuum/Oven Cured; ASTM D3039-95 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T700 12K BW Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |