Tensile Modulus 4.93 GPa
715 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RZ006SXP PA 66
LNP* THERMOCOMP* RZ006SXP is a compound based on Nylon 66 resin containing 30% Milled Glass. Added feature of this material is: Heat Stabilized.
Tensile Modulus 4.93 GPa
715 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RZ006SXP PA 66 (Asia Pacific)
LNP* Thermocomp* RZ006SXP is a compound based on Nylon 66 resin containing Milled Glass.
Tensile Modulus 4.93 GPa
715 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL FE1410PW PPE+PS (Europe-Africa-Middle East)
Noryl* FE1410PW resin is a blend of polyphenylene Oxide (PPO) and polystyrene (PS) resin that contains 10% glass reinforcement. The resin is suitable for injection molding. Noryl FE1410PW resin has ..