Polymer Property : Tensile Modulus = 728 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 5.02 GPa
728 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP KFP032 Acetal Copolymer
LNP LUBRICOMP* KFP032 is a compound based on Acetal Copolymer resin containing 10% Glass Fiber, 15% PTFE/Silicone. Added feature of this material is: Wear Resistant.
Tensile Modulus 5.02 GPa
728 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP WF002 PBT
LNP* THERMOCOMP* WF002 is a compound based on PBT containing 10% Glass Fiber.