Mechanical Properties Metric English Comments
Tensile Modulus 5.03 GPa
730 ksi
ASTM D638
Quadrant EPP Techtron® PSGF PPS - Compression Molded 40% Glass Reinforced Polyphenylene Sulfide (ASTM Product Data Sheet)
Tensile Modulus 5.03 GPa
730 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM CRS5711 PEI
15% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing.
Tensile Modulus 5.03 GPa
730 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM CRS5711 PEI (Asia Pacific)
15% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing.
Tensile Modulus 5.03 GPa
730 ksi
ASTM Test
Styrolution Terblend® N NG-04 20% Glass Filled ABS/PA6 (Dry)
Terblend N NG-04 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, low mold shrinkage and high heat resistance.Information provided by STYROLUTION, which is a joint ven..
Tensile Modulus 5.03 GPa
730 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP WF002 PBT
LNP* THERMOCOMP* WF002 is a compound based on PBT containing 10% Glass Fiber.
Tensile Modulus 5.03 GPa
730 ksi
ASTM D638
Ensinger XP-151 Compression Molded PI Compound, 15% Graphite Filled, Premium Grade
The XP 150 Series are amorphous high performance polyimides with high permanent temperature and creep resistance, as well as excellent bearing and wear properties, and excellent long term thermal st..
Tensile Modulus 5.03 GPa

@Temperature 22.8 °C
730 ksi

@Temperature 73.0 °F
ASTM D638
Quadrant EPP Duratron® PAI T7530, Compression Molded Carbon Fiber Reinforced Polyamide-Imide
Tensile Modulus 5.03 GPa

@Temperature 22.8 °C
730 ksi

@Temperature 73.0 °F
ASTM D638
Quadrant EPP Duratron® PAI T7530, Compression Molded Carbon Fiber Reinforced Polyamide-Imide