Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 5.09 GPa
738 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC (Asia Pacific)
LNP* Lubricomp* DX98306H is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible.