Mechanical Properties Metric English Comments
Tensile Modulus 5.31 GPa

@Temperature 150 °C
770 ksi

@Temperature 302 °F
ISO 527-2
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Typical applications include ..
Tensile Modulus 5.31 GPa
770 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Lubri-Tech™ BB-10GF/5T PC/ABS Blend, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Modulus 5.31 GPa
770 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66
LNP* LUBRICOMP* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
Tensile Modulus 5.31 GPa
770 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66 (Asia Pacific)
LNP* Lubricomp* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.
Tensile Modulus 5.31 GPa

@Temperature 175 °C
770 ksi

@Temperature 347 °F
4; ISO 527-2
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Dry)
Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre..
Tensile Modulus 5.31 GPa

@Temperature 150 °C
770 ksi

@Temperature 302 °F
4; ISO 527-2
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp..
Tensile Modulus 5.31 GPa
770 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Xenoy® 1760E PBT+PC
11% Glass Reinforced alloy. Impact/chemical resistant. Excellent physical property retention in automotive exteriors. High flow version of Xenoy 1760 resin.
Tensile Modulus 5.31 GPa
770 ksi
ASTM D638
Ensinger Tecapeek® XP-96 Compression Molded PEEK
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Tensile Modulus 5.31 GPa
770 ksi
ASTM D638
Ensinger Tecapeek® XP-96B Compression Molded PEEK, Unfilled, Black Pigmented
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Tensile Modulus 5.31 GPa
770 ksi
Transverse direction; ISO 527
Azdel Plus U421-B01 42% Directionalized Continuous Fiber Mat / PP Resin Matrix
AZDEL® U421-B01 is a glass mat thermoplastic laminate based upon a combination of random oriented continuous fiber mat and oriented fiber mat contained within a polypropylene resin matrix. This co..
Tensile Modulus 5.31 GPa

@Temperature 175 °C
770 ksi

@Temperature 347 °F
ISO 527-2
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength..
Tensile Modulus 5.31 GPa

@Temperature 150 °C
770 ksi

@Temperature 302 °F
ISO 527-2
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer
Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp..