Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 538 GPa | 78000 ksi | |
Toho Tenax Besfight® G80-600 12K UMA-5C F301 Continuous Filament Carbon Fiber High Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Carbon .. |