Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.450 - 0.550 GPa
65.3 - 79.8 ksi
ISO 527-2
Borealis BD212CF Polypropylene Copolymer
BD212CF is a heterophasic copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: BD212CF is designed for food packaging, l..
Tensile Modulus 0.450 - 0.550 GPa
65.3 - 79.8 ksi
ISO 527-2
Borealis BD712CF Polypropylene Copolymer
BD712CF is a heterophasic copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: BD712CF is recommended for food packaging..