Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.515 GPa @Temperature 60.0 °C |
799.9 ksi @Temperature 140 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66
(Unverified Data**) 25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR70G25V0 NC010 is a 25% glass fiber reinforced heat stabilized flame retardant polyamide 66 resin for injection molding.Information provided .. |