Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.0580 GPa | 8.41 ksi | ISO 527 |
Lubrizol ESTANE® GP95AB Ester Based Thermoplastic Polyurethane Type: Estane® GP 95AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in .. |
|||
Tensile Modulus | 0.0580 GPa | 8.41 ksi | 1 mm/min |
Arkema Group Pebax® MX 1205 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness.. |