Tensile Modulus 57.0 GPa
8270 ksi
Goodfellow Iron 78/Boron 13/Silicon 9 Alloy
Information provided by Goodfellow.
Tensile Modulus 57.0 GPa

@Temperature 80.0 °C
8270 ksi

@Temperature 176 °F
Tensile Warp, Wet; Pr EN 2561
Hexcel® HexFlow® RTM 120/HY 2954 120°C Epoxy System for RTM Two Component System
RTM 120/HY2954 is a two component system, developed for the manufacture of high performance Aerospace and Industrial composite parts using the Advanced Resin Transfer Moulding Process.
Tensile Modulus 57.0 GPa

@Temperature 23.0 °C
8270 ksi

@Temperature 73.4 °F
0°, Conditioning: 23°C; ASTM D3039
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, HTA
Fiber Designation: C193PW, Plain weaveInformation provided by HexCel
Tensile Modulus 57.0 GPa
8270 ksi
90º, RT, Dry; EN2561
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 45% 46280 Fiber
Information provided by HexCel